Tefzel? HT-2170 乙烯四氟乙烯共聚物 DuPont Fluoropolymers 产品说明: DuPont? Tefzel? fluoropolymer HT-2170 resin combines the chemical and high-temperature resistance of Tefzel? with antistatic levels of electrical conductivity. Tefzel? HT-2170 and the other Tefzel? fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared to other fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties. Tefzel? HT-2170 can perform successfully in applications where other thermoplastics are lacking in mechanical toughness, broad thermal capability, ability to meet difficult environmental conditions, or limited by fabricating problems. Properly processed products made from neat Tefzel? HT-2170 are inert to most solvents and chemicals, hydrolytically stable, and weather-resistant. The recommended upper service temperature is 150°C (302°F); useful properties are retained at cryogenic ranges. Mechanical properties include outstanding impact strength, cut-through, and abrasion resistance. The main advantage of Tefzel? HT-2170 is that it has improved stress crack resistance and flexibility when compared to other static-dissipating Tefzel? ETFE resins. To gain stress crack resistance, some physical strength has been sacrificed. Typical End Products Tefzel ? HT-2170 resin can be used to manufacture extruded tubing, pipe, and other profiles for hose; linings of components used in the chemical processing industries; industrial film; injection and blow-molded articles requiring superior electrical, chemical, and thermal properties and stress crack resistance. Tefzel? HT-2170 物性表 基本信息 特性 导电高 ESCR(抗应力开裂)共聚物抗溶剂性抗撞击性,高良好的柔韧性良好耐磨损性耐化学性良好耐气候影响性能良好韧性良好水解稳定 用途 薄膜衬里吹塑成型应用管道管道系统管件型材 形式 粒子 加工方法 吹塑成型管路挤出成型挤出树脂传递成型型材挤出成型压缩模塑注射成型 物理性能 额定值 单位制 测试方法 比重 1.70 g/cm3 ASTM D792 熔流率(熔体流动速率) (297°C/5.0 kg) 2.3 g/10 min ASTM D3159 机械性能 额定值 单位制 测试方法 抗张强度 (23°C) 27.6 MPa ASTM D638 伸长率 (断裂, 23°C) 200 % ASTM D638 热性能 额定值 单位制 测试方法 熔融温度 220 到 250 °C ASTM D3418 较高使用温度 150 °C UL 746 电气性能 额定值 单位制 测试方法 体积电阻率 1 7.0 ohms·cm ASTM D257 补充信息 Weather and Chemical Resistance: Excellent